| current position:Home >> Products |
|
| |
|
 |
|
| Name:Plates from Steels Designated for Heat Treatment |
| Item NO.YYGSP11 |
| Content: |
| Standard: |
EN 10083 |
| Plates: |
Plates from Steels Designated for Heat Treatment |
| Details: |
|
|
|
MATERIAL DIMENSIONS
|
|
Marking
|
Material Number
|
Dimensions[mm]
|
|
Thickness
|
Width
|
Length
|
|
2 C 45
|
1.1191
|
2-150
|
1000-3000
|
12000
|
|
2 C 60
|
1.1221
|
2-150
|
1000-2000
|
12000
|
|
25 Cr Mo 4
|
1.7218
|
3-150
|
1000-2000
|
8000
|
|
42 Cr Mo 4
|
1.7225
|
3-200
|
1000-2500
|
10000
|
|
CHEMICAL COMPOSITION
|
|
Marking
|
Material Number
|
Content of Elements - Mass [max%]
|
|
C
|
Si
max
|
Mn
|
P
max
|
S
max
|
Cr
|
Mo
|
|
2 C 45
|
1.1191
|
0.42-0.50
|
0.40
|
0.50-0.80
|
0.035
|
0.035
|
max 0.40
|
max 0.10
|
|
2 C 60
|
1.1221
|
0.57-0.65
|
0.40
|
0.60-0.90
|
0.035
|
0.035
|
max 0.40
|
max 0.10
|
|
25 Cr Mo 4
|
1.7218
|
0.22-0.29
|
0.40
|
0.60-0.90
|
0.035
|
0.035
|
0.90-1.20
|
0.15-0.30
|
|
42 Cr Mo 4
|
1.7225
|
0.38-0.45
|
0.40
|
0.60-0.90
|
0.035
|
0.035
|
0.90-1.20
|
0.15-0.30
|
|
MECHANICAL PROPERTIES NORMALISED CONDITION
|
|
Marking
|
Min. yield strength ReH 1] [MPa]
for thick.[mm]
|
Tensile strength Rm[MPa]
for thick[mm]
|
Min. Ductility A[%]
|
|
≤16
|
≤100
|
≤250
|
≤16
|
≤100
|
≤250
|
≤16
|
≤100
|
≤250
|
|
2 C 45
|
340
|
305
|
275
|
620
|
580
|
560
|
16
|
16
|
16
|
|
2 C 60
|
380
|
340
|
310
|
710
|
670
|
650
|
10
|
11
|
11
|
|
25 Cr Mo 4
|
380
|
-
|
550
|
600
|
-
|
850
|
~22
|
~22
|
~22
|
|
42 Cr Mo 4
|
600
|
-
|
800
|
750
|
-
|
1000
|
~15
|
~15
|
~15
|
|
Normalising of these steels improves workability without affecting hardenability
|
|
|
|
| |
|
|
|
|
|